| Heat Treatment | Tensile Strength(N/mm2) | Elongation (%) | Reduction of Area (%) | Shore Hardness | Yield Point (kg/mm2) | |
|---|---|---|---|---|---|---|
| 78.5Parmalloy | No Treatment | 45~50 | 40~45 | 65~70 | 38~40 | 20~28 |
| Quench to 600~700°C After 1000°C anneal | 60~70 | 20~25 | 40~50 | 38~40 | 30~40 |